Hony Engineering Plastics Co.,Ltd.
Hony Engineering Plastics Co.,Ltd.
Ev> Macal> German Rochling Gray Durostone CFR767

German Rochling Gray Durostone CFR767

May 18, 2023

German Rochling Gray Durostone CFR767


CFR767-3


The combination of processing cycles in high temperature environments combined with aggressive fluxes can cause degradation of standard Durostone grades.

The solution is Durostone CFR767, which is specially formulated for aggressive fluxes and high temperature process configurations.

The resin used to produce Durostone CFR767 can withstand temperatures up to 300°C. When the solder bath temperature exceeds 265°C and the bottom PCB preheat exceeds 140°C, Durostone CFR767 should be used instead of the standard grade.

Durostone CFR767 has excellent flux resistance. When fluxes containing halides or dicarboxylic acids are used in high-volume production, the lifetime of standard grade materials is reduced, so Durostone CFR767 is the ideal solution.

Bizimlə əlaqə saxlayın

Author:

Ms. Tina

Phone/WhatsApp:

+8618680371609

Populyar Məhsullar
Şirkət xəbərləri
Blog News
What Is PEEK Ball ?

November 13, 2024

PVDF Application Areas

November 03, 2024

You may also like
Related Categories

Bu təchizatçıya e-poçt göndərin

Mövzu:
Mobil telefon:
E-poçt:
Mesaj:

Your message must be betwwen 20-8000 characters

Bizimlə əlaqə saxlayın

Author:

Ms. Tina

Phone/WhatsApp:

+8618680371609

Populyar Məhsullar
Şirkət xəbərləri
Blog News
What Is PEEK Ball ?

November 13, 2024

PVDF Application Areas

November 03, 2024

Sizinlə əlaqə saxlayacağıq

Daha çox məlumat əldə edə bilməsi üçün daha çox məlumatı doldurun

Məxfilik Bəyanatı: Məxfiliyiniz bizim üçün çox vacibdir. Şirkətimiz şəxsi məlumatlarınızı açıq icazənizlə hər hansı bir genişləndirməyə və ya açıqlamamağı vəd edir.

Göndər